Browsing by Subject Ni-base superalloys
Showing results 1 to 1 of 1
Issue Date | Title | Author(s) |
---|---|---|
28-Nov-2016 | Effect of superficially applied Y2O3 coating on high-temperature corrosion behavior of Ni-base superalloys | Goyal, G.; Singh, H.; Singh, S.; Prakash, S. |